Are you doing just carbon SAW or is it multiple processes I.E. Alloys....
Ans: Yes sir, we manufacture Carbon Steel pipes only.
Second question are you using multiple fluxs? i.e. chemical composition
Ans: We have two kinds of Flux: Agglomerated (Basic) and Fused (all imported)
One other thing you mentioned your own recycling efforts.....does the supplier offer any incentives or anything related to re manufacture.......if not do other suppliers offer that consideration?
Ans: The idea of recycling the slag came from the flux supplier. That practice went well (about 15 to 20 years) and saved a lot of production cost until it was stopped few years ago.
I brought this issue to seek answers, maybe some have a better idea related to waste management. Sad to say, were not an ISO 14001 certified.
Thanks Tommyjoking for your research efforts.
Are Aye