Hey all,
Thanks for the responses.
Lawrence,
Yes C10 was much better. I am playing around with different mixes to find an optimal process. Even though no one recommends C2, I wanted to see what it would produce.
Phil,
Yes I tried 98 Ar/2 O2 (SG-AO 2%). It wetted out nicely.
Al,
So you have no problems welding with SG-AC-2% ?
Tyrone