Hello all
Is mandatory show the brand manufacturer to filler metal on PQR and WPS ?? AWS D1.5 Bridge Welding Code
Thank for your advice
Miguel Teran
By
Steelslinger
Date
07-19-2018 19:49
Table 5.2 (D1.5-2015 Edition) specifies the requirement, and Commentary-5.5.1 has a more in depth explanation of the issue.
By
MIGUEL TERAN
Date
07-23-2018 06:52
Thank ....I appreciate your information
Topic
AWS.org
/
Forum News & Help
/ AWS D1.5 Bridge Welding Code / Filler Metal
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill