cmshone & SS,
Welcome to the Original AWS Welding Forum.
Go to the SSAB website or Google "welding Hardox" for a pdf of recommendations.
SS is correct for using low(er) strength filler, unless you need the weld to be wear resistant.
Above all, use low hydrogen process and procedures.
Tyrone