Dear All,
kindly suggest me the pressure drop in 1.6 mm drill hole when we pressurize 206 Kg/cm2 with 16 sec holding.
the data given below.
Pipe Diameter - 323.9 mm
Wall thickness - 7.35 mm
Pipe length - 12.12 Meter
Drill Hole size - 1.6 mm
Pipe Pressure Hold - 206 Kg/Cm2
Holding time fro pressure - 16 Sec
Regards,
Apoorva Mehta