I am currently a second year welding student at MTI in Mitchell, South Dakota. While going through the AWS code book, version 2015 I came across a question; why in 4.22.3.2 does it say that one shall conform to 6.12.2 except 6.12.2.2. shall not apply?
Parent - By Steelslinger (**) Date 10-11-2018 15:35
If you look at what is allowed for discontinuities, you would see that Tension (6.12.2.1) criteria and Compression (6.12.2.2) criteria have different levels of what is acceptable. So with that, you will be able to see why one is excluded and also understand why the Code differs to the one it does.