We have a D1.8 project, which requires that the electrodes meet diffusible hydrogen requirements for H16, per Appendix W in the AISC Seismic Specification. I'm aware of three different designators... H4, H8, and H16. Im thinking that H4 or H8 will meet H16, but can someone please verify this?