QW-403.10 mentions, " for the short-circuiting transfer mode of the gas metal-arc process, when the qualification test coupon thickness is less than 1/2 in, an increase in thickness beyond 1.1 times that of the qualification test coupon."

is this mean only for groove weld or both for groove & fillet weld?

for example, when the thickness is 1.0mm,
1) groove weld: 1.0~1.1mm  and fillet: unlimited
2) groove weld: 1.0~1.1mm  and fillet: 1.0~1.1mm