- - By qa1 Date 01-30-2019 16:23
Can we use a multigrade steel A588/A709 gr. 50 for qualification of welder?
Parent - - By jwright650 (*****) Date 01-30-2019 16:27
What welding code are you working with?
Parent - - By qa1 Date 01-31-2019 15:03
AASHTO/AWS D1.5. Bridge Welding Code
Parent - By jwright650 (*****) Date 01-31-2019 15:35
D1.5 has a few things to watch for when qualifying welders:

Clause 5.21.3 Base metal has to be an AASHTO approved steel as described in Clause 1.2.2 or the WPS(see Clause 5.24.1.1)

Clause 5.24.1.1
If the project has steel with 90ksi yield or greater, it makes you qualify on base metal meeting the same specification as the steel for the project.
Parent - By Steelslinger (**) Date 01-31-2019 21:12
A588/A709-50W is listed as M270 under AASHTO.

We use it extensively for our D1.5 welder qualifications as we work primarily on Weathering Steels.