- By LToca85 (**) Date 02-14-2019 22:35
Hello all, in D1.6 2017 6.7.1 and 6.7.2 it states that for CJP welds (6.7.1)  and PJP welds (6.7.2) test taken in any position qualifies the procedure for any position. My dilemma is that it has zero mention on what position will qualify for witch position for fillet welds, or maybe I just don't see it. I am also having a hard time grasping 6.7.1 and 6.7.2 as they state that qualifications of CJP qualify PJP and fillets and qualifications of PJP qualify fillets. Am i misinterpreting that or is that really what it says?