By Sa3idy
Date 02-24-2019 03:46
Edited 02-24-2019 03:53
Thanks a lot, is there any para. at ASME IX Support me for that ?
If the As Run Sheet (Monitoring Sheet) not mention the root and cap height , what is the Thickness to be reduced for root and cap?
Example :
I have PQR Support GTAW and SMAW, Base Metal Thickness 18 mm, but At (as run sheet and PQR) GTAW deposit weld metal 5 mm and SMAW deposit weld metal 18 mm (not mention root and cap height). what is the Thickness of deposit weld metal to be qualified for each process?