Hi all,
I have a WPS that is approved with Back gouging,can i use the same WPS to qualify my welders without Backing/Back gouging ?
According to AWS D1.1
If you look at Table 4.12 I don't think you can.
To weld without backing or backgouge you will first need s WPS that is qualified via clause 4.
You may then quality your welders (performance) with that.
Yes, you are right.
"When welding arc spot welds, what decrease in welding current(amperage), wire feed speed or melting rate is permitted, without using another WPS?
a. None
b. 5%
c. 7%
d. 10%
Dear Friends
i have WPS in EN Standard for shell with nozzle fit up as set-on type.
can i use the same wps for set-in type ?