Up Topic Welding Industry / General Welding Discussion / Fillet wps as per API 1104
- - By vignesh5585 (*) Date 05-03-2019 06:06
Hey guys,

How to qualify fillet procedure qualification as per API 1104 and from where i can get dia and thickness qualification ranges. Please give reference clause so that i can prepare my proposed wps as 1104.
Parent - - By Jim Hughes (***) Date 05-03-2019 19:38
Vignesh,
If you have an API1104 21st edition it's found in paragraph 5.7 and Fig. 10.
Hope that helps
Parent - - By vignesh5585 (*) Date 05-16-2019 02:10
As per clause 5.7 it has not clearly stated about diameter and thickness qualification.
Parent - By 803056 (*****) Date 05-16-2019 02:18
API 1104 is a little iffy. They refer to a branch with a CJP groove weld as a fillet. So, I have to have clarification as to what you really want, a branch that is CJP with a reinforcing fillet weld or a real fillet weld?

Al