Hi Ilkin
The essential variables for Procedure qualification are found in Table 4.5, 4.6 & 4.7 depending on process or CVN requirements.
The essential variables for Performance qualification are found in Table 4.12.
The short answer I think is No.
However there can be restrictions on Maximum fillet size and there can be restrictions on weaves vs stringer beads when CVN's are required (table 4.6) which can have an impact on number of beads produced in a weldment.
Having said that... If bead sequence or number of beads are important for the fabrication of whatever it is you are making, you can of course place that requirement into your WPS and that makes it essential for the welder to follow.
If you say a little more about your situation and why you ask the questions, I think you will get much better feedback.