I have a project with X-42 to X-65 pipe grades.

If a welder test on the X-65 WPS does he / she also have to test to weld to the X-52 WPS? 

I know in 1104 pipe grade is an essential variable for procedure qualifications but for welder qualifications only OD and WT are essential variables.
Parent - By Shane Feder (****) Date 06-04-2019 23:15
No, not required.
The only essential variable you have to be aware of is a change in filler material classification (if any)
Cheers,
Shane