We need to replace the amp/volt meter we use to calibrate welding machines. Which one do you use, and what do you like about it? I'm looking for a good, inexpensive one.
Parent - By Steelslinger (**) Date 07-08-2019 19:28
We use two Flukes (I410 Clamp Current Meter & 179/EFSP Multimeter) and a Weschler D Tong Test Ammeter. Its what our maintenance dept. has and uses.
Parent - - By SeeJeepGo (*) Date 07-22-2019 12:25
Parent - By SWN1158 (***) Date 07-22-2019 13:05
Thanks !