Regardless of the code allowances, if the WPS indicates plate only, the it would have to be revised, a new one written, or a new one qualified.
In some codes, plate procedure qualification tests would qualify a WPS for pipe. But if that WOS indicated plate only, then you could not use that WPS for pipe until the WPS indicates so.