By bigmac
Date 11-11-2019 12:34
hello all , quick question from a newbie, we havean AWS D1.1 weld procedure done in the 6G position, does this cover us for K connectios as well or do we have to run another procedure to cover this
You didn't mention whether you are using the same welding process, filler metal F number, wall thickness, or material group. How can we say you are good to go if you changed the welding process?
Al
By bigmac
Date 11-11-2019 15:20
hello AI , yes all the same, just want to know if a standard 6G butt covers a K weld
The PQR must use a restriction ring.
Al