AWS D1.1 is not set up to qualify more than one process on a single test plate. This differs from ASME or AWS B2.1 where the thickness range is based on the thickness of the deposit as well as the thickness of the test coupon. AWS D1.1 is based on the thickness off the coupon exclusively. That being the case, how would you determine the qualified thickness range of each process based on D1.1?