Up Topic Welding Industry / General Welding Discussion / Laser Welding Depth Penetration
- - By kdawg119 Date 12-06-2019 03:21
When laser welding is conducted on a plate, the penetration depth seems to increase when the laser is near the edge of the plate. I don't understand why?
Parent - By 803056 (*****) Date 12-06-2019 15:23
Reduced thermal mass?

Al