Morning Lawrence,
I'm in agreement, however let's dig a little deeper.
Where exactly are you seeing the thicknesses qualified in Table 4.10?(positions only)
Table 4.11 gives the ranges qualified for plate testes, but doesn't mention positions, so can you use two different thicknesses as long as one of the tests is with 1" or greater material to qualify for unlimited thicknesses?
I saw this question earlier and it made me look twice at this, because I had just always went with 1" materials on all of the testing as it seemed like more bang for the buck to me.
Edit: I guess the answer is in the Figures listed rather than in the text of the code, as they specify limited thickness and unlimited thickness qualifications