Atuuel,
Quickest answer is yes, it is required. A couple of questions. 1. What is the diameter? 2. what is the configuration? i.e. double jointed pipe, or is it pipe to fitting? 2. Are you required to back gouge or back grind to sound metal? I'm going to give a response but need more info. Since it's pipe it should be fairly easy to place high heat purge balloons in the pipe, (depending on the answer to question 1 is) build a dam in the pipe with rice paper, or just purge the pipe during welding. Last option could be ceramic tape to be used as backing. Gulco makes a very good product.