- - By Atuuel (*) Date 06-04-2020 17:10
Hi everyone,

As max. 5% Fe is need to be achieved in Inconel 625 weld overlays.

Cant this limit be relaxed to some more iron percentage by compromising corrosion resistance and reducing some equipment life.

As lots of technology, resources, special consumables are required to achieve this chemistry.

I have read some articles where there was mentioned about this limit. But further work is still pending in this direction.
Parent - By Jim Hughes (***) Date 06-06-2020 13:04
That is an engineering, failure analysis (a process to prove what you are saying is correct) and client question.