Gentlemen,
I’m looking for an instrument for testing welding gas, mainly Co2. (75%-25%).
I have a Bacharach FYRITE gas analyzer and it is not very accurate or consistent.
Any suggestions?
By
Lawrence
Date
08-12-2020 17:11
I was able to borrow an "Oxy Baby" from my local Airgas rep...
It was super easy to use at the end of the gun & at connections.
It was calibrated and accurate to a 10th of a percent... Which was good enough for my welding gas issue.
https://www.oxybaby.com/application/?gclid=EAIaIQobChMI35_73JOW6wIVicDACh3L_gt5EAAYASAAEgIwafD_BwE
By
Jim Hughes
Date
08-12-2020 20:03
Thanks very much Lawrence. I looked it up and it looks very good. Good to know someone that used it and it worked.
Topic
Welding Industry
/
General Welding Discussion
/ Test instrument for testing 75%-25% welding gas
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Technical Standards & Publications
- Conferences & Shows
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Welding Fundamentals
- Processes
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill