Hi everyone,
Can I know the PWHT temperature and soaking time of a particular weld can be decided based upon the weld metal PWHT requirements as mentioned in ASME Sec 2 Part C.
For example, I am using a base metal SA335 P11 grade 4" sch 40 pipe weld with E8018-B2 welding rod SMAW process. The PWHT can be selected according to ASME Sec 2 part C as, SFA 5.5, E8018-B2 PWHT for 690 plus or minus 15 degree celcius for 1 hour soaking. Is this correct the correct way