- - By Pallawit Dubey Date 01-12-2022 02:50 Edited 01-12-2022 02:53
What shall be minimum holding time for PWHT as per UCS 56-1 of ASME Sec VIII Div I for nominal thickness of 53 mm. (Is PWHT minimum holding time required to be calculated based on “15 min/in.” factor for each additional inch i.e. Is interpolation allowed while calculating like e.g. for 53 mm the minimum holding time = 120+15x0.11811=121.772 minutes=122 minutes ?)
Parent - - By Jovi Zhu (**) Date 02-03-2022 13:02
Hi, I believe you are calculating the right way.
Parent - By Pallawit Dubey Date 06-15-2022 08:48
Ok Sir. Thanks