- - By binhjack (*) Date 03-19-2022 03:44
Is it required to check the the bevel/ groove angle after backgouging during the WPS qualification process in accordance with AWS D1.1? What clause mentioned?

Thank you in advanced.
Parent - By 803056 (*****) Date 03-19-2022 18:45
It would depend on the edition you are using. Regardless of the edition, there is a clause that states back gouges should resemble a prequalified J-, or U-groove. Now, if you are taking the position that you are qualifying the WPS to establishing the minimum contour of a back gouge, you can do so, just make sure you record the data on the PQR.

Al