By Toey TNDT
Date 10-11-2022 05:55
Edited 10-11-2022 06:06
Dear Expert
As API 660 requires a Micro-hardness test with comply Nace Standard
I suspected in ASTM E384 and hardness survey point of NACE MR0175
how to micro-hardness(tiny point) provide the correct requirement
Micro-hardness may be pressed at pearlite or bainite. ?
Regards