I understand the requirements of Fillet Weld testing in accordance with Figure 6.15 of AWSD1.1 (Fillet Weld Soundness Tests for WPS Qualification. What I'm struggling with is, if I produce a test piece with a single fillet one side and a multipass fillet the other side, can they both be included in the one PQR, to qualify a single pass WPS and a multipass WPS?
Thanks
Bryan