I am looking over a new job that was sold and I'm reading through the contract specs and it states....
"Qualifications for welding work: Qualify welding processes and welding operators in accordance with AWS "Standard Qualification Procedure".
Provide certification that welders to be employed in work have satisfactorily passed AWS qualification tests within the previous 12 months."
Ok, I know I've been down this same road a time or two with you guys and I value your opinions and when I see something that reads out of the norm, I start to wonder exactly what they want for us to do.
1) Does this first sentence want us to qualify per D1.1 section 4 just like we've always done or are they asking for us to do something different, I haven't seen it worded quite that way before(AWS " Standard Qualification Procedure")
2) Does the second sentence ask us to requalify anyone who has a qualification record older than 12 months?
Any help is always appreciated, I usually try to read too much into this stuff rather than taking it for what it says :)
John Wright