WHAT IS THE MAX.FILLET WELD SIZE FOR SAW DUEL ELECTRODE PER D11.THANK YOU. SINGLE PASS
Parent - - By Bill Mc (**) Date 03-24-2005 13:47
Just an FYI since I'm not positive about D1.1, but the AWS Bridge Code D1.5 specs a max of 1/2" for single pass, multiple electrode, horizontal fillet weld.
Parent - By mksqc (**) Date 03-24-2005 17:25
CWB W47.1 5\16 is the max.pre qual. fillet size.I thought AWS D11 was the same but if im reading table 3.7 correctly the max pre qual.is 1\2'' would like to get comfermation if possible.
Parent - By swnorris (****) Date 03-24-2005 17:30
Per D1.1, using multiple electrodes, 1/2" fillet welds in the horizontal position is prequalified.