/ Hobart or Lincoln SMAW rods?
By
RODTESTER
Date
04-06-2005 20:33
I have used both but want your view. I am useing them in a repair shop and need to know what the pros and cons of each are. I am useing 7010, 7018, 7024, 8010.
By
TimGary
Date
04-07-2005 12:00
I've found the Hobart rods to be 100% as good as Lincoln while at the same time 10 - 15% cheaper in price.
Tim
Topic
Welding Industry
/
General Welding Discussion
/ Hobart or Lincoln SMAW rods?
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill