That's a DIN material, so you should search in Germany or Switzerland first of all.
I would guess that the material belongs to the blades, so, if I were you, the first thing I would do was to get in contact with the turbine manufacturer to buy the spare parts and have a recommendation on how to do the welding job.
Giovanni S. Crisi
Sao Paulo - Brazil