![](/mwf/attachments//avatars/4269-2369.jpg)
Question for the forum, but some background first...
I have read AWS D1.1:2004 Paragraph 7.4.5.
Our bent plate came in bent incorrectly with the horizontal leg over hanging the centerline by 1" of a beam flange that will get (31) 3/4" dia. studs shot down the centerline. I made a few people upset by getting the fitter to trim that extra 1" of the entire length of plate(roughly 30feet) to allow the studs to be shot in the correct location on the flange (on the centerline of the web), when they had already told the fitter to not worry with it and let it go. I don't think they liked me questioning their decision, but I wanted it done right.
Could I have let that go and still be within the requirements of paragraph 7.4.5? I was wondering how the EOR would have felt about it structurally.
John Wright