Welder qualification "Table 4.8 positions qualified" Three questions. When a welder qualifies on a groove weld on plate in the 3G position is he qualified for the 1G, 2G, 3G, 1F, 2F, 3F, as well as pipe 24" dia and above for these same positions?
If the welder qualifies to a wps in the 3G & 4G table 4.8 says he/she is qualified for All positions. Does this include 6GR also?
If the welder fails one of these test positions either the 3G or the 4G, could he not be considered qualified for the position that he/she did pass?
Thank You for your help,