- - By Matt Date 04-12-2001 13:11
I'm looking for references on welding titanium to steel, either directly or using a plate of intermediate material suitable for welding to each. Are any conventional methods available?

Matthew H. Ferry
Crucible Research Center
mferry@crucibleresearch.com
Parent - By TimGary (****) Date 04-12-2001 14:09
Titanium cannot be welded to other metals with any process other than explosive bonding, as far as I know...
Parent - By G.S.Crisi (****) Date 04-16-2001 22:17
Get in touch with the titanium top specialists in the world, The Titanium Company of America. They're very kind people and will give you every assistance you need. Their site is www.timet.com
Giovanni S. Crisi
Sao Paulo - Brazil