I'm in general agreement with the technique recommendations here. We do nothing but GTAW and GMAW-Spray, the techniques mentioned for GMAW are the same ones we use here. When I was a young pup, maybe 30 years ago, I learned to GMAW weld using the drag technique, it was a hard habit to break but virtually every "expert" I've spoken to recommends the push technique, for a variety of reasons.