By -
Date 10-17-2005 15:38
Bill,
I'm sorry. The carbon content of the C-1010 is such that it is not considered a high carbon. My mistake. According to the AISI specifications, such steels as C1008, C1010, and C1020, etc, refer to the carbon content. The carbon content of these steels do not exceed 0.08, 0.10, and 0.20% respectively.