Military Standard for Fusion Welding for Aerospace Applications
"The scope of this document is to provide minimum requirements for weld filler materials, workmanship, inspection and record requirements for fusion welding of alloys applicable to aircraft, missiles, other aerospace equipment, their parts and accessories."
thank you.could you be more specefic. what I mean is if you were told to weld 6061 alum to mil-std- 2219. what would that tell you.
Val,
In a number of areas AWS D17.1 has superseeded that specification. This is also true of MIL-STD-1595 You might check into this before you do too much more work.
Gentlemen,
where can I buy the MIL standards, apart from the US Secretary of Defense?
Any distributor, bookstore?
Thankyou for the reply
Giovanni S. Crisi
Sao Paulo - Brazil
Giovanni,
Don't know if you can buy the military standards, but here's a link to D17.1
http://www.techstreet.com/cgi-bin/detail?product_id=957620
Thank you, Gentlemen. Of course, I would like to know the standards just for scholar purposes.
Giovanni
Giovani
I was surprised to find Mil Std 1595 at Global Engineering.
Apparently you have been granted top secret clearence by Mr. Rumsfeld :)
http://global.ihs.com/doc_detail.cfm?currency_code=USD&customer_id=21254D2D2E0A&shopping_cart_id=28255827244B40484A5A3D3C3C0A&country_code=US&lang_code=ENGL&item_s_key=00069769&item_key_date=120500&input_doc_number=mil%201595&input_doc_title=
http://global.ihs.com/doc_detail.cfm?currency_code=USD&customer_id=21254D2D2E0A&shopping_cart_id=28255827244B40484A5A3D3C3C0A&country_code=US&lang_code=ENGL&item_s_key=00069769&item_key_date=120500&input_doc_number=mil%201595&input_doc_title=
By -
Date 11-10-2005 21:51
Lawrence,
Like most of the MIL standards, MIL-STD-1595 is available for free download on the World Wide Web. It has been superseded by AMS-STD-1595, however, as of June 1998.
Mankenberg
from MIL-STD 2219A-2005 :
4.2 Welding procedure qualification-
Prior to engaging in production welding, the welding procedure for Classes A and B shall be qualified. The pertinent welding variables shall be identified. Section 2 of AWS B2.1 should be used as a guideline in the development of the welding procedure to ensure that all pertinent variables and tolerances are included. Requalification criteria shall be determined by the cognizant engineering organization.
4.3 Welding personnel qualification-
Each welder or welding operator shall be qualified in accordance with AWS D17.1 section 4 prior to performing any production welding.