We machine 12L14 which rusts very easy. In the past pre-braze we have dipped the parts in a rust preventative product. However, this contaminates the braze joint. We are looking for a process or chemical that is braze friendly that will protect the part from rusting. Our braze house does not process the parts for a few weeks. We pre-assemble the joint with BAg-13a shims so cleaning the part pre-assembly, assembling then dipping in rust preventative is not an option. We have had good success tumbling with a 2% soap solution and not rinsing completely and blowing off the residue but this is very time consuming. Any solutions available??