As long as you are talking about F numbers and P numbers, don't overlook the A number when working with either ASME or AWS D2.1. The A number is the chemical analysis of the weld deposit. The A numbers apply to ferrous metals and are grouped based on chemistry of the diluted weld deposit.
Good luck - Al