Has anybody got any documentation on sizinf a flare-bevel weld with a reinforcing fillet? I need to weld a tube to a plate, and the flare bevel weld isn't strong enough, but I don't know how much credit I can take for the reinforcing fillet.
By
henri
Date
12-28-2005 00:04
In D1.1 see prequalified joint BTC-P10 etc..refer to note 7 and also refer to sections 2.3.2.7 and 2.6.4 (last sentence is important)
Topic
Welding Industry
/
Technical Discussions
/ Sizing flare-bevel with reinf. fillet
Forum
AWS.org
- Forum News & Help
American Welding Society Services
- Certifications
- Conferences & Shows
- Technical Standards & Publications
- AWS Learning & Education
Welding Industry
- General Welding Discussion
- Technical Discussions
- Inspection & Qualification
- Processes
- Welding Fundamentals
- ASME Codes
- Welding Safety
- Metallurgy
- Welding Documents & Downloads
Welders and Inspectors
- Education & Training
- Welding Equipment Classifieds
Sections
- Section 7: San Francisco
- Section 32: Rochester
- Section 39: Colorado
- Section 41: Puget Sound Olympic
- Section 55: Arizona
- Section 81: Nebraska
- Section 110: North Florida
- Section 112: Florida West Coast
- Section 135: Nevada
- Section 156: Inland Empire
Chit-Chat & Non-Welding Discussion
- Off-Topic Bar and Grill
Powered by
mwForum
2.29.2 © 1999-2013 Markus Wichitill