Up Topic Welders and Inspectors / Education & Training / Jaeger No. 1 and 2 chart
- - By Jameslu Date 02-23-2006 08:18
All personnel that perform visual and dimensional inspection of weldments shall be trained and qualified.
An annual eye exam of Jaeger 1 shall be given to each trained and qualified inspector.
For welder, apply Jaeger no. 2 chart.

What is Jaeger no. 1 and 2 chart?
Any example?
Parent - By QCCWI (***) Date 02-23-2006 10:52
It is an eye chart. It has several paragraphs of different sizes. The inspector or welder has to be able to read the paragraph at a certain distance. ASNT sells the chart.
Parent - By tito (**) Date 02-23-2006 12:27
Go to asnt.com and then browse around and look for the "shop asnt" link. Once there, do a search for "jaeger", or "visual acuity". The are available for $8.65. I just looked this stuff up two days ago so its fresh on my mind.
Parent - By thcqci (***) Date 02-27-2006 16:07
This is where I got my charts http://www.west-op.com/visactes.html