Hello
May be this is to late with my comments but sometimes may help
removing conventional spring-insert from the torch & changing onto the new one with teflon guide also - the current tip of the torch shall be changed more frequently,
besides I like better 2%CO2 than 2%O2.
Improoving goes good with pulsed GTAW - 90Hz, basis ca100, peak150.