- - By mnelson (*) Date 03-16-2006 17:12
Anybody have any welding experiences with E9015-G? We have a new reheater going in one of our boilers that has SA 213 T23 tubing. Our installer has recommended the E9015-G over E9018-B3.
Parent - By GRoberts (***) Date 03-16-2006 20:27
By itself, the AWS classification 9015-G means nothing as far as the chemical analysis of the electrode. The -G means that the chemical anlysis is to be agreed upon between the purchaser and supplier. Better get more information on what the rod actually consists of.