Reading about E-7018 Downhand? topic (july 14,00), I am traing to know if that kind of considerations apply to E-6010 as well.
We have an internal spec. wich say taht it only apply vertical down.
the weldment will be for a 36" Dia 1" thk. API X52 welding in 6G position. the WPS indicate the root pass will be made uphill & the other beds downhill. I'm traing to know the best technical consideration and its support?