Regards, everyone. At the moment I'm trying to develop a GMAW procedure to spot weld two overlapped 1/8'' AISI 1020 sheets. The upper sheet has a 5 mm diameter hole, in whose center the wire is positioned. How could I start trying (parameters, pre and post gas shielding, welding time, etc...). I could already notice in preliminar tries that either intern or extern central cavity (by the way, what would be the technical term for that?) is very difficult to get over.