- By involute Date 04-04-2006 02:29
we are manufacturing some bushes in C45 steel and they have to be welded onto mild steel or ST52 steel
The joint is getting cracked after welding
the process is being done by MIG welding
please let me know what welding wire is to be used and what precautions are to be taken