- - By Rich68 Date 02-03-2006 00:37
Figured I'd move my question to its own post.

I have a Trindl 125A, which is a 125 Amp, 110/220v unit.

I have a question for the group: While the unit is in mint condition, the cables have been lost. What are the proper cable ends for those (roughly) 1/8" sockets?

Thanks.
Parent - By 357max (***) Date 02-04-2006 18:00
I have a 125 Trindl and replaced the receptacles and plugs with Miller's old Thunder-Bolt machine type. Red, Black, Yellow & White gives me a visual setting. I use the machine as a sacrifice to break up the magnetism on oil field pipe for corrals & feed bunks. I just run the AC through magnetic oil field pipe while welding it with a DC machine.
Parent - - By Aussie Date 04-14-2006 05:34
I have acquired a Trindl 125A and the casing has had a hard life - all the markings have disappeared. Is there any place I can get a front sticker to show what the different plugs are? If not can someone tell me what the settings are so I can get some idea of how to connect the plugs correcly for different welding jobs.
Any help will be appreciated.
Thanks
Parent - - By Rich68 Date 04-14-2006 14:23
I not only have the front sticker, I have the manual for mine, which I can scan and e-mail to you, just give an e-mail address, and I can do it next week.

In the meantime, here's the chart (I hope the formatting works):

A B C D
1 20 23 26 30
2 35 40 45 50
3 55 60 65 70
4 80 95 110 125
Parent - - By Aussie Date 04-14-2006 15:33
Thanks Rich for the informatiom. The manual will be a great help. You can email a copy to FXHolden@msn.com
Is the left bank of terminals ABCD or 1234?
Much appreciated!!
David
Parent - - By Rich68 Date 04-14-2006 16:39


1-4 on left A-D on right.

I will have access to a scanner next week, and will e-mail you with the manual then.

-Rich
Parent - - By H60Gunner Date 03-01-2008 19:08
Any chance I could get a copy of this manual as well?  I just recently aqquired a trindle 125a for free and would like to know more about it.
Parent - By H60Gunner Date 03-01-2008 19:23
if anyone still monitors this board my email is placenciar@hotmail.com