I would like to know how viable underwater welding is, in other words how much underwater welding is there, and how much of a demand is there? Thinking about going to commercial dive school for "wet" welding. Any info would be helpful. Thanks
Is demand jobs, but limited works. Wet welding actully is not establish as dry welding processes. Hyperbaric welding is always done to get sound and good mechanical intergrity.